302HQ Stainless Steel: High-Quality Austenitic for Fasteners
Aug 05, 2025
Palik žinutę



What defines 302HQ's chemical composition?
It contains 17-19% chromium, 8.5-10.5% nickel, 3-4% manganese, and carbon <=0.06%. The balanced alloying and low carbon enhance cold formability, critical for shaping bolts, screws, and nuts without cracking.
How does 302HQ perform in cold working?
302HQ excels in cold heading and threading, with high ductility that allows for severe deformation during fastener production. It work-hardens gradually, maintaining toughness even after extensive cold forming.
It offers corrosion resistance similar to 304, performing well in atmospheric conditions and mild chemicals. The low carbon content reduces the risk of intergranular corrosion, making it suitable for outdoor fasteners.
How does 302HQ compare to 304 in applications?
302HQ replaces 304 in fastener production, where its superior cold formability prevents cracking during threading. 304 remains better for structural parts needing higher tensile strength.
Where is 302HQ commonly used?
Found in high-quality bolts, screws, and nuts for automotive, construction, and electronics. It's also used in precision fasteners requiring consistent performance and corrosion resistance.