AISI 316L Stainless Steel 2B Finish Cold Rolled Sheet
Oct 30, 2025
Palik žinutę
If you are looking for high-quality, corrosion-resistant stainless steel sheet for industrial, chemical, or marine applications, AISI 316L cold-rolled 2B stainless steel sheet is an ideal choice.
GNEE's AISI 316L stainless steel sheet, produced through a cold-rolling process, ensures precise thickness and flatness, and features a uniform, semi-bright finish. Maintaining excellent hygiene standards, it is ideal for machining, forming, and polishing, making it suitable for applications such as chemical storage tanks, heat exchangers, and marine equipment.
What is the difference between 316 and 316L stainless steel sheets?
316L has a lower carbon content (<0.03%) than 316, which reduces carbide precipitation, improves weldability, and enhances its corrosion resistance in high-temperature and corrosive environments.
316L Cold Rolled Stainless Steel Sheet (2B Finish)
| AISI 316L / EN 1.4404 / SUS316L | |
| 2B Finish (Smooth, uniform, semi-bright) | |
| 0.3 mm – 6.0 mm (customizable) | |
| 1000 mm – 2000 mm (customizable) | |
| 2000 mm – 6000 mm (customizable) | |
| <= 0.4 μm | |
| 515–720 MPa | |
| Yield Strength (0.2% offset) | >= 205 MPa |
| >= 40% | |
| 8.0 g/cm³ | |
| -196℃ to +870℃ | |
| ASTM A240 / ASME SA240 / EN 10088 / JIS G4304 |
Price Range: Typically USD 4.50 – 7.50 per kg depending on thickness, width, quantity, and surface finish.
Minimum Order Quantity (MOQ): 500 kg (custom orders possible)
Lead Time: 7–15 days for standard stock, longer for customized dimensions.
Certifications: ISO 9001, SGS, BV; Mill Test Certificates (EN 10204/3.1B) available.
Packaging: PE protective film, waterproof paper, wooden crates, or as per customer specification.

Q: Which industries use 316L cold-rolled steel sheets?
A: Commonly used in the chemical, shipbuilding, food processing, pharmaceutical, and construction industries.
A: Yes. 2B surface treatment maintains a smooth surface after shearing, laser cutting, and bending, minimizing surface defects.
Q: Are customization and value-added services offered?
A: Yes. We can provide custom sizing, precision cutting, polishing, deburring, and packaging services according to customer requirements.
Siųsti užklausą






